Technical Data
Ti-6Al-2Sn-4Zzr-6Mo (Ti-6-2-4-6)
Ti-6-2-4-6 was developed to combine the high temperature properties of 6-2-4-2 with higher strength. It is used in gas turbine applications, discs, propellers and also for sour well applications.
Chemistry Limits (%) |
|
Al | 5.5 - 6.5 |
Sn | 1.75 - 2.25 |
Zr | 3.50 - 4.50 |
Mo | 5.50 - 6.50 |
O2 Max | 0.15 |
Fe Max | 0.15 |
H2 Max | 0.0125 |
C Max | 0.04 |
N2 Max | 0.04 |
Mechanical Properties |
|
Guaranteed Minimum | Duplex Annealed Condition |
Ultimate Tensile Strength - ksi | 160 - 170 |
Yield Strength - ksi | 150 - 160 |
Elongation % | 6-10 |
Physical Properties |
|
Density (lbs/in3) | 0.168 |
Elastic Modulus (x106 psi) | 16.5 |
Beta Transus Temp (oF) | 1710 |
Weldability | Limited |